Observation Examples of Thin Film

Agregar marcador

Observation of Coated Video Tape

Observation of Coated Video Tape

Changes in the magnetic powder-coated surface caused by the ambient humidity were observed. The acicular ratio of the magnetic powder seems to drop when the humidity is increased. These changes cannot be observed with metal-evaporated tape and so it is possible that they are caused by the binder. (A temperature and humidity controller was used.)
(Data provided by Sony Corporation)