Observation Examples of Polymers
Observation of Laminated Plastic

Topographic Image (above) & LFM Image (below)
The sample is grasped by the holder, a cross section produced, and observed. With the LFM image the cross section layer structure appears from large and small friction forces caused by the difference in molecular weights.