Observation Examples of Living Organisms

Agregar marcador

Observation of Primary Cultures of Nerve Cells

Observation of Primary Cultures of Nerve Cells

These images show nerve cells taken from the dorsal root ganglion of a rat. The observation specimens were prepared by (1) cultivating the nerve cells on a glass substrate, (2) fixing them with paraformaldehyde, (3) cleaning them with distilled water, and (4) air-drying them. The extended rod-shaped protrusions and bumps on the cell surfaces can be seen clearly.